OUR NEW PHONE NUMBER IS BELOW, PLEASE CALL IF YOU HAVE ANY QUESTIONS 714-362-7456
Cart 0
2 #12 Mabor (MgO) Cupels 3.16"x1.85" Gold-Assay-Smelting-Refining 354 Grams lead
2 #12 Mabor (MgO) Cupels 3.16"x1.85" Gold-Assay-Smelting-Refining 354 Grams lead
2 #12 Mabor (MgO) Cupels 3.16"x1.85" Gold-Assay-Smelting-Refining 354 Grams lead
2 #12 Mabor (MgO) Cupels 3.16"x1.85" Gold-Assay-Smelting-Refining 354 Grams lead
2 #12 Mabor (MgO) Cupels 3.16"x1.85" Gold-Assay-Smelting-Refining 354 Grams lead
2 #12 Mabor (MgO) Cupels 3.16"x1.85" Gold-Assay-Smelting-Refining 354 Grams lead
2 #12 Mabor (MgO) Cupels 3.16"x1.85" Gold-Assay-Smelting-Refining 354 Grams lead
2 #12 Mabor (MgO) Cupels 3.16"x1.85" Gold-Assay-Smelting-Refining 354 Grams lead
Make Your Own Gold Bars.com

2 #12 Mabor (MgO) Cupels 3.16"x1.85" Gold-Assay-Smelting-Refining 354 Grams lead

Regular price $35.00 $0.00 Unit price per
Tax included. Shipping calculated at checkout.

Each Cupel will absorb approximately 354.4 grams of lead .

Cupels are made from high quality dead burnt magnesia (MgO). Hard, smooth surface with consistency in weight and size. Provide exceptional results in gold mines, precious metal refiners, alloy melters, hallmarking, geological and test laboratories worldwide. Each crucible will be wrapped in paper and shipped in a box

CUPEL DIMENSION DATA (mm / inches)
D – 80.2 / 3.16
D1 – 57.5 / 2.26
D2 – 62.5 / 2.46
H – 47.0 / 1.85
H1 – 16.5 / 0.65

Weight: 443.0g Approx.


The lead button for cupellation is typically generated in the crucible fusion from the fire assay process, but can also be produced by a scorification assay, or a bullion assay where the precious metal is wrapped in lead foil.

Typical cupellation furnace temperatures in gold and silver assays are 1650-1700F, but can vary with technique, air flow volume, and cupel material.